EarlyCompressiveStrength
- V1.1
ActiveClass property
Context
| Data template (PDT) | Cement V1.0 |
|---|---|
| Group of properties | performance data |
| Class property id | 4071 |
|---|---|
| URI (class property) | https://pdts.pt/uri/0.1/classprop/4071-ResistenciaACompressaoInicialEDeReferencia |
| URI (property) |
https://pdts.pt/uri/0.1/prop/ResistenciaACompressaoInicialEDeReferencia
Version: https://pdts.pt/uri/0.1/prop/ResistenciaACompressaoInicialEDeReferencia/v1 |
| GUID | aabc8a7b44bd46349dc77767b8f0ac84 |
| Name | Compressive strength (early and standard) |
| Description in this class | Compressive strength class of the cement, expressed in terms of strength classes and limits, covering both early strength and standard strength. Essential characteristic under EN 197-1:2011 Table ZA.1, clauses 7.1, 8, 9. |
| Definition | Compressive strength class of the cement, expressed in terms of strength classes and limits, covering both early strength and standard strength. Essential characteristic under EN 197-1:2011 Table ZA.1, clauses 7.1, 8, 9. |
| Units | MPa |
| Data type | String |
| Status | Active |
| Version | 1 |
| Revision | 1 |
| Date of revision | 2026-09-22 |
| Date of version | 2026-09-22 |
| Reference document | n/a |